| Description | A new type of interface treatment material composed of small particle size modified polymer emulsion, multi-functional additives and other materials. Improves the quality of the overall coating of the wall. |
| Main Ingredient | Acrylic copolymer emulsion, pigments, additives and water |
| Construction method | Brush, roller |
| Environment | Temperature > 8°C, Relative humidity < 85%. |
| Recoat Time | At least 2 hours (extended in winter). |
| Dilution | Water weight ratio max 10%. Stir evenly before use. |
| Theoretical Area | 8~12m2/kg/layer (varies by wall roughness). |