1 / 5
| Customization: | Available |
|---|---|
| Appearance: | Powder |
| Color: | Gray |
| ITEM | Technical Parameters |
|---|---|
| Water-cement Ratio | 0.25:1 |
| Product Status | Gray or white powder |
| Construction Temperature | 5-35℃ |
| Operational Time | 2hrs |
| Opening Hours | 15min |
| Time to bear load | ≥24hrs |
| Reference dosage | 1.5kg/m2·mm |
The wall must be clean and solid, no hollow, no mold release agents, no wax stains. Painted surfaces should be rough chiseled to expose at least 80% of the original surface. Newly plastered surfaces should maintain for at least 7 days before tiling.
Mix tile glue with water in proportion (20kg powder: 4.5-5kg water). Add water first, then pour the powder. Stir well with an electric mixer until smooth.
Scraping method with trowel for double-sided (for smooth wall) or traditional paste method (for uneven surfaces).
It can be used for plastering, concrete, brick wall covering, ceramic tiles, ceramic mosaics, and small natural stone installations.